Abstract
Mongolia has a few regions rich in precious metals with well known examples being Oyu-Tolgoi, Erdene Mongol and Boroo Gold. One of these deposits is the Salkhit gold and silver deposit which is the focus of this study. This study utilizes Salkhit gold and silver samples for metallurgical testing to determine the practicality of these undertakings. The experiments focus on comparing and potentially combining metallurgical methods of flotation and leaching to see what yields greater results. Another focus of this study is to explore the usage of an alternative gold leaching medium, glycine, which has gained popularity worldwide as a safer alternative compared to the default medium of cyanide. Head grades were not uniform across the sample suite as a consequence of combining ores from the two deposits. The A33 sample (33% gold ore) returned grades of 0.27 ppm Au and 25.5 ppm Ag, while the A66 sample (66% gold ore) returned 1.29 ppm Au and 5.0 ppm Ag. Mineralogical analysis confirmed that both ore types are dominated by quartz and muscovite gangue, with gold hosted in arsenopyrite and pyrite, and silver occurring as acanthite, freibergite–tetrahedrite, bornite, and chalcopyrite. In this study head samples from Salkhit East deposit primary source of gold and the Salkhit secondary deposit primary source of silver were sent and mixed in different ratios these being 1:1, 1:2, 2:1 for simplicity's sake they'll be referred to as Au:Ag mix or 50:50, A66 and A33. These mixed samples were ground to a P80 of 106 μm, followed by flotation tests. These tests aimed to determine the ideal reagent usage and evaluate the most effective mixing ratios for optimal beneficiation. Copper sulfate at a dosage of 600 g/t had the best outcome as an activator. The optimal pH value was 9.0, reached with the addition of lime. OTZ at a dosage of 50 g/t as a frother, and for collectors either ADD, SBX, or Aero 8045 at a dosage of 100 g/t worked well. The optimal mixing ratio for Au:Ag in closed-circuit flotation was determined to be 2:1, achieving 79.7% gold recovery and 68.1% silver recovery, outperforming the 1:1 ratio (77.4% Au, 44.7% Ag) and the 1:2 ratio (78.8% Au, 33.1% Ag). It can be seen in the results that gold recovery doesn't vary much with the mixing ratios, but silver is affected the most. For the leaching portion of the experiment, variously mixed head samples along with tailings from the flotation tests were leached with glycine and cyanide then evaluated. Glycine leaching was conducted with the temperature set to 60 °C, pH of 11 and stirring speeds of 400 rpm with 0.5M of glycine while cyanide leaching temperatures were set to 40 °C, pH of 11.15 and stirring speeds of 400 rpm with 1M NaCN. The pH was adjusted using NaOH. Glycine achieved greater gold recovery than cyanide head samples at mixing ratios of 2:1 and 1:2 reaching 93.28% and 94.33% respectively. In contrast, cyanide leaching for the same mixing ratios only reached 56.85% and 30.14% gold recovery, with much greater results on flotation tailings, the best one being for a 1:2 mix reaching 92.59% gold recovery. The results suggest higher yields on flotation tailings especially for cyanide leaching.
Description
Keywords
Gold and silver processing, Leaching, Glycine leaching, Flotation